  "name": "Ceramic processing stages: material state, options named and main constraint",
  "description": "Original compilation of the six processing stages of sintered technical ceramics, the state of the material at each stage, the options a manufacturer names, and the main constraint, built from CeramTec's manufacturing process page and the UNSW and Penn State explanations of ceramic hardness and brittleness.",
  "page": "https://casrai.org/guides/ceramic-processing",
  "publisher": "CASRAI",
  "license": "https://creativecommons.org/licenses/by/4.0/",
  "dateModified": "2026-11-19T14:11:04Z",
  "temporalCoverage": null,
  "spatialCoverage": null,
  "columns": [
    {
      "name": "Stage",
      "unit": "",
      "description": ""
    },
    {
      "name": "State of the material",
      "unit": "",
      "description": ""
    },
    {
      "name": "Options or checks named by the source",
      "unit": "",
      "description": ""
    },
    {
      "name": "Main constraint",
      "unit": "",
      "description": ""
    }
  ],
  "rows": [
    {
      "Stage": "Powder and mass preparation",
      "State of the material": "Powder",
      "Options or checks named by the source": "Grinding, mixing, granulating, drying",
      "Main constraint": "Grinding influences later properties"
    },
    {
      "Stage": "Shaping",
      "State of the material": "Green body, low strength",
      "Options or checks named by the source": "Isostatic and axial pressing, injection moulding, extrusion, tape or slip casting, 3D printing",
      "Main constraint": "Body is shaped but not yet solid"
    },
    {
      "Stage": "Green machining",
      "State of the material": "Green body, low strength",
      "Options or checks named by the source": "Milling, turning, drilling, laser cutting",
      "Main constraint": "Relatively easy and cost-effective because of low strength"
    },
    {
      "Stage": "Debinding and sintering",
      "State of the material": "Compacted and solidified at high temperature below melting point",
      "Options or checks named by the source": "Pressureless or pressure-assisted; continuous or discontinuous; air, inert gas or vacuum",
      "Main constraint": "Debinding may need a separate step, e.g. aluminium nitride"
    },
    {
      "Stage": "Finishing",
      "State of the material": "Sintered, high strength",
      "Options or checks named by the source": "Grinding, lapping, polishing, lasering",
      "Main constraint": "Machining after sintering is much more complex"
    },
    {
      "Stage": "Final inspection",
      "State of the material": "Sintered part",
      "Options or checks named by the source": "Dimensions, surface, cracks, porosity; visual, measurement, sometimes non-destructive testing",
      "Main constraint": "Brittle fracture from flaws: toughness about fifty times lower than metals"
    }
  ],
  "sources": [
    {
      "title": "CeramTec: Manufacturing process of high-tech ceramics",
      "url": "https://www.ceramtec-group.com/en/high-tech-ceramics/manufacturing-process",
      "accessed": "2026-11-19"
    },
    {
      "title": "UNSW Materials Science: Properties of ceramics",
      "url": "https://www.unsw.edu.au/science/our-schools/materials/engage-with-us/high-school-students-and-teachers/online-tutorials/ceramics/properties",
      "accessed": "2026-11-19"
    },
    {
      "title": "Penn State MATSE 81: What is a brittle material?",
      "url": "https://courses.ems.psu.edu/matse81/node/2106",
      "accessed": "2026-11-19"
    }
  ]
}