  "name": "Fracture-surface features by failure mode",
  "description": "Compiled from three failure-analysis sources: PACE Technologies' failure analysis guide, Xometry's fractography resource and a 2019 ASM Advanced Materials & Processes fatigue case study. Each row lists the macroscopic or whole-specimen features and the microscopic features the sources associate with a failure mode. Qualitative descriptions only; no source gives numeric cut-offs.",
  "page": "https://casrai.org/guides/fractography",
  "publisher": "CASRAI",
  "license": "https://creativecommons.org/licenses/by/4.0/",
  "dateModified": "2026-11-26T08:15:00Z",
  "temporalCoverage": null,
  "spatialCoverage": null,
  "columns": [
    {
      "name": "Failure mode",
      "unit": "",
      "description": ""
    },
    {
      "name": "Macroscopic or specimen-level features",
      "unit": "",
      "description": ""
    },
    {
      "name": "Microscopic fracture-surface features",
      "unit": "",
      "description": ""
    },
    {
      "name": "Sources",
      "unit": "",
      "description": ""
    }
  ],
  "rows": [
    {
      "Failure mode": "Ductile",
      "Macroscopic or specimen-level features": "Necking and reduction in cross-sectional area; cup-and-cone surface; plastic deformation in the microstructure",
      "Microscopic fracture-surface features": "Dimpled appearance at high magnification, from microvoid growth and coalescence",
      "Sources": "PACE Technologies; Xometry"
    },
    {
      "Failure mode": "Brittle",
      "Macroscopic or specimen-level features": "Flat, featureless surface; minimal plastic deformation in surrounding material",
      "Microscopic fracture-surface features": "Cleavage facets in crystalline materials; river patterns; intergranular features",
      "Sources": "PACE Technologies; Xometry"
    },
    {
      "Failure mode": "Fatigue",
      "Macroscopic or specimen-level features": "Beach marks (macroscopic bands); multiple crack initiation sites; progressive crack growth; final fast-fracture region",
      "Microscopic fracture-surface features": "Striations (microscopic); aligned striations characteristic of fatigue",
      "Sources": "PACE Technologies; Xometry; ASM Advanced Materials & Processes (2019)"
    },
    {
      "Failure mode": "Creep",
      "Macroscopic or specimen-level features": "Time-dependent deformation; elongated grains in the direction of stress",
      "Microscopic fracture-surface features": "Grain boundary cavitation; intergranular fracture surface",
      "Sources": "PACE Technologies"
    }
  ],
  "sources": [
    {
      "title": "PACE Technologies: Failure Analysis",
      "url": "https://metallographic.com/guides/failure-analysis",
      "accessed": "2026-11-16"
    },
    {
      "title": "Xometry: Fractography: Definition, Methods, and Failure Analysis",
      "url": "https://www.xometry.com/resources/materials/fractography/",
      "accessed": "2026-11-16"
    },
    {