  "name": "GaN wafer routes: dislocation density and reported diameter by growth route",
  "description": "Compares four routes to a gallium nitride wafer by typical dislocation density, wafer diameter reported in the cited sources, and device role. Compiled from five open-access peer-reviewed papers read on 2026-11-20; values are as reported, not normalised across suppliers.",
  "page": "https://casrai.org/guides/gallium-nitride-wafer",
  "publisher": "CASRAI",
  "license": "https://creativecommons.org/licenses/by/4.0/",
  "dateModified": "2026-11-24T12:20:00Z",
  "temporalCoverage": null,
  "spatialCoverage": null,
  "columns": [
    {
      "name": "Route",
      "unit": "",
      "description": ""
    },
    {
      "name": "Substrate and growth",
      "unit": "",
      "description": "How the wafer is made"
    },
    {
      "name": "Typical dislocation density",
      "unit": "cm^-2",
      "description": "As stated in the cited paper"
    },
    {
      "name": "Diameter reported in source",
      "unit": "",
      "description": ""
    },
    {
      "name": "Role stated in source",
      "unit": "",
      "description": ""
    }
  ],
  "rows": [
    {
      "Route": "GaN on silicon",
      "Substrate and growth": "Thin GaN film on a silicon wafer",
      "Typical dislocation density": "about 10^9",
      "Diameter reported in source": "up to 200 mm purchasable; 300 mm HEMT demonstrated",
      "Role stated in source": "Lateral devices such as HEMTs; low-cost large-area route"
    },
    {
      "Route": "Free-standing HVPE GaN",
      "Substrate and growth": "0.5-2 mm GaN film grown on sapphire or GaAs over about 5-20 h, then separated",
      "Typical dislocation density": "10^6 to 10^7",
      "Diameter reported in source": "not stated in source",
      "Role stated in source": "Native substrate for laser diodes and vertical devices"
    },
    {
      "Route": "Ammonothermal bulk GaN",
      "Substrate and growth": "Supercritical ammonia growth on GaN seeds; boule sliced into wafers",
      "Typical dislocation density": "10 to 100 times fewer than HVPE",
      "Diameter reported in source": "2 inch",
      "Role stated in source": "Best reported quality; vertical power devices"
    },
    {
      "Route": "Engineered CTE-matched substrate (QST)",
      "Substrate and growth": "8.5 um GaN on a polycrystalline AlN core",
      "Typical dislocation density": "not given as one figure in source",
      "Diameter reported in source": "200 mm",
      "Role stated in source": "CMOS-compatible vertical GaN power devices"
    }
  ],
  "sources": [
    {
      "title": "Key et al., Structural and Electrical Characterization of 2in Ammonothermal Free-Standing GaN Wafers, Materials 2019",
      "url": "https://pmc.ncbi.nlm.nih.gov/articles/PMC6630438/",
      "accessed": "2026-11-20"
    },
    {
      "title": "Goncalez Filho et al., Thick GaN drift layers on 200 mm CTE-matched substrate, Scientific Reports 2023",
      "url": "https://pmc.ncbi.nlm.nih.gov/articles/PMC10517926/",
      "accessed": "2026-11-20"
    },
    {
      "title": "AlGaN HEMT structures grown on miscut Si(111) wafers",
      "url": "https://pmc.ncbi.nlm.nih.gov/articles/PMC10303388/",
      "accessed": "2026-11-20"
    },
    {
      "title": "May et al., Diamond thin films: a twenty-first century material. Part 2",
      "url": "https://pmc.ncbi.nlm.nih.gov/articles/PMC12059586/",
      "accessed": "2026-11-20"
    }
  ]
}