  "name": "INCONEL alloy 718 limiting composition read against superalloy element roles",
  "description": "Limiting composition ranges (weight percent) for INCONEL alloy 718 from the producer data sheet, paired with the role each element plays in nickel superalloys as described in the Cambridge materials science notes and Carpenter Technology selection guidance. Compiled by combining the data sheet with the two role sources; rows without a stated minimum are maximum limits only.",
  "page": "https://casrai.org/guides/nickel-superalloy",
  "publisher": "CASRAI",
  "license": "https://creativecommons.org/licenses/by/4.0/",
  "dateModified": "2026-11-18T15:09:20Z",
  "temporalCoverage": null,
  "spatialCoverage": null,
  "columns": [
    {
      "name": "Element",
      "unit": "",
      "description": ""
    },
    {
      "name": "Minimum",
      "unit": "wt %",
      "description": ""
    },
    {
      "name": "Maximum",
      "unit": "wt %",
      "description": ""
    },
    {
      "name": "Role in nickel superalloys",
      "unit": "",
      "description": ""
    }
  ],
  "rows": [
    {
      "Element": "Nickel (plus cobalt)",
      "Minimum": 50,
      "Maximum": 55,
      "Role in nickel superalloys": "Base of the nickel-base class (more than 50% Ni); gamma matrix and Ni3(Al,Ti) gamma-prime"
    },
    {
      "Element": "Chromium",
      "Minimum": 17,
      "Maximum": 21,
      "Role in nickel superalloys": "Essential for oxidation resistance; solid-solution strengthener; carbide former"
    },
    {
      "Element": "Iron",
      "Minimum": "balance",
      "Maximum": "balance",
      "Role in nickel superalloys": "Solid-solution strengthener; the balance element in 718"
    },
    {
      "Element": "Niobium (plus tantalum)",
      "Minimum": 4.75,
      "Maximum": 5.5,
      "Role in nickel superalloys": "Forms niobium-rich gamma-double-prime hardening phase; strain-hardens matrix"
    },
    {
      "Element": "Molybdenum",
      "Minimum": 2.8,
      "Maximum": 3.3,
      "Role in nickel superalloys": "Solid-solution strengthener; carbide former"
    },
    {
      "Element": "Titanium",
      "Minimum": 0.65,
      "Maximum": 1.15,
      "Role in nickel superalloys": "Essential gamma-prime solute (with Al); carbide former"
    },
    {
      "Element": "Aluminium",
      "Minimum": 0.2,
      "Maximum": 0.8,
      "Role in nickel superalloys": "Essential gamma-prime solute; aids oxidation resistance"
    },
    {
      "Element": "Cobalt (maximum)",
      "Minimum": "not specified",
      "Maximum": 1,
      "Role in nickel superalloys": "Solid-solution strengthener"
    },
    {
      "Element": "Carbon (maximum)",
      "Minimum": "not specified",
      "Maximum": 0.08,
      "Role in nickel superalloys": "Carbide former"
    },
    {
      "Element": "Boron (maximum)",
      "Minimum": "not specified",
      "Maximum": 0.006,
      "Role in nickel superalloys": "Grain-boundary strengthener"
    }
  ],
  "sources": [
    {
      "title": "Special Metals: INCONEL alloy 718 data sheet (SMC-045)",
      "url": "https://www.specialmetals.com/documents/technical-bulletins/inconel/inconel-alloy-718.pdf",
      "accessed": "2026-11-18"
    },
    {
      "title": "University of Cambridge: Superalloys",
      "url": "https://www.phase-trans.msm.cam.ac.uk/2003/Superalloys/superalloys.html",
      "accessed": "2026-11-18"
    },
    {
      "title": "Carpenter Technology: Selection of Age-Hardenable Superalloys",
      "url": "https://www.carpentertechnology.com/blog/selection-of-age-hardenable-superalloys",
      "accessed": "2026-11-18"
    }
  ]
}