ASTM F1140 is a standard test method for measuring how well a package withstands internal pressurization when nothing physically restrains it. It has a burst procedure, which pressurizes the package until it fails, and a creep procedure, which holds a specified pressure for a specified time or until failure. A companion method, ASTM F2054, does a similar burst test with the package held between restraining plates. This page is general information about what the methods cover, not medical advice or a test procedure.
What ASTM F1140 covers
The full title is “Standard Test Methods for Internal Pressurization Failure Resistance of Unrestrained Packages”. The ASTM store (checked 2026-11-01) lists the current designation as F1140/F1140M-13(2025), active, last updated 22 October 2025. An earlier edition, F1140-07(2012), is now marked historical, so a test report may cite an older edition than the one in force.
The standard states that its purpose is determining the ability of packages to withstand internal pressurization. ASTM describes the use as a rapid way to assess the likelihood of failure when a package is exposed to a pressure difference, such as during sterilization and transportation, and says it can be used in manufacturing and across the package life cycle. The SI and inch-pound versions are each standard in their own right and are used independently.
The standard text itself is sold by ASTM, so this page paraphrases the published scope and significance statements and does not reproduce test pressures, rates, dwell times or acceptance limits. Those values are not given here, and the standard should be read directly before specifying a test.
Burst versus creep
Burst test
In the burst procedure the package is pressurized until it fails. The question it answers is how much internal pressure the package took before failure.
Creep test
In the creep procedure a specified pressure is applied for a specified time, or until the package fails. The question it answers is whether the package holds a chosen pressure for a chosen duration. A testing laboratory’s own descriptive summary (Intertek, checked 2026-11-01) splits creep into a pass/fail version (a specified pressure for a specified time) and a time-to-failure version; that split is the laboratory’s description rather than wording from the ASTM pages.
F1140 versus F2054 versus F88
The three methods are often requested together and are easy to confuse. The table below uses only statements from the ASTM F1140 and F2054 scope and significance sections.
| Method | What it does | What the standard says it cannot tell you |
|---|---|---|
| ASTM F1140 (unrestrained packages) | Burst or creep testing by internal pressurization of a package that is not held between plates | Results do not necessarily correlate with seal strength measured by Test Method F88; F2054 says F1140 may not reliably detect the weakest area of the seal |
| ASTM F2054 (restraining plates) | Determines the minimum burst strength of a perimeter seal on a flexible package pressurized within restraining plates, which keep the shape stable so stress spreads more evenly along the seal | It is an indicator of burst strength; it does not measure seal uniformity or overall package integrity, and its results may not correlate with F1140 or F88 |
| Seal strength by ASTM F88 | Referred to in both standards as a separate seal-strength measure | Neither standard promises that its result tracks the F88 result |
The practical reading is that these are three different questions. A package can be reported against one method and say little about the others, so a supplier’s “passed ASTM burst testing” needs the method number attached.
F2054 is the current edition F2054/F2054M-13(2024), active, last updated 15 November 2024, per the ASTM store (checked 2026-11-01).
Why results differ between labs
F1140 states that results from different equipment correlate only if all the relevant parameters match, including package size, material, seal configuration, test equipment, the rate of air flow into the package, machine sensitivity and the position of the test article. F2054 adds plate rigidity and plate spacing for its own equipment comparisons. Two reports with the same headline number can therefore describe different conditions.
What to ask for in a test report
This checklist turns the standards’ own comparability statements into questions. It is a reading aid built from those statements, not a requirement written by ASTM.
- Which method and which edition does the report cite (for example F1140-13(2025) or an older F1140-07(2012))?
- Was the test burst or creep, and for creep, what pressure and time were specified?
- What package size, material and seal configuration were tested, and do they match the package you will actually use?
- Were restraining plates used (F2054) or not (F1140), and if plates were used, what were their rigidity and spacing?
- What airflow rate and equipment were used, so the result can be compared with another laboratory’s?
- Does the report claim anything about seal uniformity or overall package integrity? F2054 says its burst result does not measure either, so integrity claims need a different method. See USP 1207 package integrity evaluation.
Where it matters for labs, clinics and supply decisions
The standards name sterilization and transportation as situations where a package sees a pressure difference. Staff who read supplier documentation for sterile or sealed packaging can use the questions above to see whether a quoted burst or creep result is comparable to another one. Related CASRAI pages cover specimen bags for biohazard transport, Packing Instruction 620 for Category A infectious substances and laboratory sealing film; those pages state their own requirements, and ASTM F1140 is not presented here as a substitute for them.
Common misunderstandings
- “A burst number is a seal-strength number.” F1140 says its results do not necessarily correlate with F88 seal strength.
- “Burst testing proves package integrity.” F2054 says its result is an indicator of burst strength and does not measure seal uniformity or overall integrity.
- “A result from one lab can be compared to any other.” Only when the listed parameters match.
- “F1140 and F2054 are interchangeable.” F2054 uses restraining plates so stress spreads more evenly around the seal, which helps find the weakest area, and says its results may not correlate with F1140.
FAQ
What does ASTM F1140 test?
The ability of a package to withstand internal pressurization while unrestrained, by a burst procedure (pressurize until failure) or a creep procedure (hold a specified pressure for a specified time or until failure).
What is the difference between ASTM F1140 and ASTM F2054?
F2054 pressurizes a flexible package within restraining plates to determine the minimum burst strength of the perimeter seal. F1140 uses no plates and, according to F2054, may not reliably detect the weakest area of the seal.
Is ASTM F1140 still current?
On 2026-11-01 the ASTM store listed F1140/F1140M-13(2025) as active.
Sources
Checked 2026-11-01.
- ASTM International, F1140/F1140M-13(2025): https://store.astm.org/f1140_f1140m-13r25.html
- ASTM International, F1140-07(2012), historical: https://store.astm.org/f1140-07r12.html
- ASTM International, F2054/F2054M-13(2024): https://store.astm.org/f2054_f2054m-13r24.html
- Intertek, Burst and Creep ASTM F1140 overview (descriptive summary only): https://www.intertek.com/polymers/testlopedia/burst-creep-astm-f1140/