Skip to main content
v2026.11,986 entries · CC-BY 4.0

Graphite Anode in Lithium-Ion Cells: How Lithium Fits Between the Layers

How a graphite anode stores lithium in LiC6 (372 mAh/g), when lithium plating starts, and what USGS 2026 figures show on supply.

Written and maintained by CASRAI Editorial Board

Published

On this page

A graphite anode is the negative electrode of most lithium-ion cells: a layered form of carbon that stores lithium by taking lithium ions between its carbon sheets during charging and releasing them during discharge. Fully lithiated graphite has the composition LiC6, one lithium ion for every six-carbon ring, which gives a theoretical capacity of 372 mAh/g. This guide covers the electrochemistry, the conditions under which lithium plates instead of intercalating, and the supply picture published by the US Geological Survey.

Definition and scope

In a lithium-ion cell the anode is the electrode where lithium sits when the cell is charged. Graphite is an allotrope of carbon, and the graphite used in cells comes in two broad forms: natural graphite, which is mined, and synthetic graphite, which is manufactured, commonly from petroleum coke (Battery University, BU-309, updated 7 May 2024). Electrode makers process either form into the powder, often called active anode material, that is coated onto a current collector.

Scope note: “graphite anode” is also used for a different object, the consumable or inert anodes used in electrolysis and cathodic protection. This page is only about the lithium-ion negative electrode. For an alternative active material that stores more lithium per gram but swells strongly, see the CASRAI guide to the silicon anode; for a cell chemistry that pairs a different anode with a sulfur cathode, see lithium-sulfur batteries.

How lithium goes into graphite

Intercalation and the LiC6 limit

During charging, lithium ions move through the electrolyte and enter the spaces between graphene layers, a process called intercalation. Chen and co-authors, writing in ACS Electrochemistry (2025, 1(5), 574-587), describe the fully lithiated end point as LiC6 with one Li+ per C6 ring and a theoretical capacity of 372 mAh/g. That number is a ceiling for the material, not a property of a finished electrode: real electrodes also contain binder, conductive additive and a current collector, and real cells are not cycled to exactly the theoretical limit.

Staging

Lithium does not fill graphite evenly. It occupies the galleries between layers in an ordered sequence called staging, in which stage 1 is the fully lithiated state and higher-numbered stages have lithium in only some of the galleries. In the operando microscopy work of Lu and co-authors (Nature Communications 14:5127, 2023), the stage colours observed in the electrode map to state of charge as follows: stage 3 near SOC 0.23, stage 2 near SOC 0.52, and stage 1 near SOC 0.95, with a dilute stage 1L appearing below SOC 0.05. In electrochemical data the transitions between stages show up as distinct peaks when the capacity-voltage curve is differentiated; Chen et al. report four dQ/dV peaks marking the staging transitions up to stage 1, where the full 372 mAh/g is reached.

Stage observed (Lu et al. 2023) State of charge (SOC)
Stage 1L (dilute) below 0.05
Stage 3 about 0.23
Stage 2 about 0.52
Stage 1 about 0.95

For a lab reader this is the practical value of a half-cell measurement on graphite: the shape of the dQ/dV curve is a fingerprint of the staging sequence, so a change in peak position or a missing peak is a diagnostic signal about the electrode, not just a change in capacity.

The first-charge surface layer

Chen et al. also report shoulders near 0.7 V during charging that they attribute to electrolyte reduction forming a “primitive SEI-like layer” on the graphite surface. The solid electrolyte interphase (SEI) is the passivating film that forms where the electrode meets the electrolyte; it consumes some lithium on the first charge and is one reason first-cycle capacity loss is measured separately from steady-state capacity.

Why fast charging and cold temperatures plate lithium

Graphite is a good anode partly because it intercalates lithium at a potential only slightly above lithium metal. The same property creates its main failure mode. Lu et al. state that “it is widely accepted that plating could occur when the anode potential falls below 0 V” (versus Li/Li+), and Chen et al. place lithium plating at graphite potentials of 0 V vs Li/Li+ and below. Plated lithium is metallic lithium deposited on the particle surface instead of lithium inside the lattice. The studies discussed here are laboratory results from specific cells; the numbers below describe those cells and are not general limits for commercial products.

Temperature

Chen et al. tracked how much charge could be passed before the graphite potential reached 0 V. In their three-electrode cells it crossed 0 V at 412 mAh/g at -20 °C, but at only 160 mAh/g at -30 °C and 106 mAh/g at -40 °C. In other words, the colder the cell, the earlier the electrode reaches the plating potential, because intercalation becomes slower relative to the charging current.

Current

In the same study, at 10 mA/cm² (about 4.13C in their cells) no intercalation peaks appeared and charging was plating-dominated. This is a statement about their electrode loading and cell design: C-rate and current density do not transfer directly between cells with different electrode thickness.

State of charge

Lu et al. combined operando microscopy with a phase-field model of the electrode (natural spherical graphite at 95.5 wt%, in 1 M LiPF6 in EC/EMC with 2 wt% vinylene carbonate). Their model fit uses a plating nucleation barrier of 20 mV, and it identifies surface saturation of lithium content (SOC about 0.98) as the prerequisite for plating onset. The model predicts that charging at 1C all the way to 100% SOC causes 17% capacity loss, which falls to 1.3% with a voltage cut-off at 75% SOC and to 0.2% at 65% SOC. For a 2 mAh/cm² electrode at 1C they predict plating can begin as early as 65% SOC. Those are model results for one electrode design; they show why charge cut-offs and temperature limits are protocol decisions, not just convenience settings.

Plating matters beyond capacity. Cells that may have been cycled hard or cold are a transport-classification and storage issue as well as a performance one; see the CASRAI guide to lithium battery shipping regulations for how cells are handled in transit.

Natural, synthetic and spherical purified graphite

The USGS Mineral Commodity Summaries 2026 chapter on natural graphite describes the main material routes into cells. Natural flake graphite is shaped and purified into spherical purified graphite (SPG), which is then used as battery anode material. Synthetic graphite powder, and secondary synthetic graphite from machining graphite shapes, compete with natural graphite in battery applications, according to the same chapter.

The distinction matters at the electrode level because the two feedstocks are different starting materials that go through different processing before they become a coated electrode. The Lu et al. electrodes, for example, used natural spherical graphite; results from one feedstock should not be assumed to carry over to another without testing.

Dry air handling matters for the electrolyte side of the cell rather than for the graphite powder itself; see the CASRAI guide to the dry room for where moisture control enters lithium-ion cell assembly.

Where it matters for labs and supply decisions

Two different questions sit under “graphite anode”: what the material does electrochemically, and where it can be obtained. A research group, a cell-testing lab or a procurement office needs both, and the USGS gives the supply side in dated figures.

  • Domestic mining. According to the USGS, no natural graphite was mined in the United States in 2025. The US consumed an estimated 71,000 tonnes of natural graphite valued at $128 million, imported an estimated 79,000 tonnes, and had 100% net import reliance in each year from 2021 to 2025.
  • Anode material imports. Imports of graphite battery anode material, natural and synthetic together, were 43,400 tonnes in the first eight months of 2025 against 28,100 tonnes in the same period of 2024. By source, China supplied 55%, Indonesia 31% and Korea 14%.
  • Concentration of mine output. China accounted for an estimated 82% of world natural graphite mine production in 2025, 1,400,000 tonnes of a 1,800,000 tonne world total (rounded). China exported 37,400 tonnes of SPG in the first nine months of 2025, up 29% from 29,100 tonnes a year earlier.
  • Domestic SPG. The USGS reports that SPG is produced in the United States by two companies, in Illinois and Louisiana.
  • Trade measures. Following a December 2024 petition, the US Department of Commerce issued preliminary determinations in 2025 of antidumping duties of 93.50% and countervailing duties of 11.58% to 721.03% on active anode material from China.
  • Reserves. The USGS lists world reserves of 310,000,000 tonnes and resources exceeding 800 million tonnes, so the supply constraints it describes concern production and processing location, not geological scarcity.

For a lab, the practical reading is narrow. The electrochemistry on this page is independent of where graphite comes from, but the feedstock type (natural or synthetic) and the processing route are properties you should record and report with any anode result, and trade measures and import reliance are reasons a published anode specification may change between purchase lots or suppliers. Neither the USGS nor the studies above give a recommendation on which supplier or form to buy, and this page does not either.

Common misunderstandings

“A graphite anode holds 372 mAh/g”

372 mAh/g is the theoretical capacity of LiC6. It describes the intercalation limit of the active material, not what a finished electrode, a full cell or a pack delivers once binders, additives, the SEI and charging limits are included.

“Plating starts at exactly 0 V”

0 V vs Li/Li+ is the widely cited threshold, but the studies above show the capacity reached before that threshold changes strongly with temperature (412, 160 and 106 mAh/g at -20, -30 and -40 °C in one study’s cells) and the model of Lu et al. includes a 20 mV nucleation barrier and a dependence on electrode loading and surface saturation. Treat 0 V as a diagnostic marker in a three-electrode cell, not a universal safe operating limit.

“Graphite and graphene are interchangeable”

Graphene is a single carbon sheet; graphite is a stack of such sheets. The intercalation described here depends on the layered stack with spaces between sheets, so the two terms should not be used as synonyms in a methods section.

“Synthetic and natural graphite give the same result”

The USGS describes them as competing for battery use, which is a statement about substitutability in the market, not about identical cell performance. The Lu et al. result was obtained with natural spherical graphite and should be cited with that qualifier.

“A graphite anode is an electrolysis anode”

The lithium-ion negative electrode and the electrolysis or cathodic-protection anode share a word and an element. Their roles, operating conditions and failure modes are different, as noted in the scope section above.

Reporting checklist for graphite anode work

The sources above point to a short list of details that change how a graphite result should be read. They are drawn from what the cited studies themselves specify.

  • Graphite type: natural or synthetic, and whether it is spherical (Lu et al. specify natural spherical graphite at 95.5 wt% in the electrode).
  • Electrolyte: composition and additives (Lu et al.: 1 M LiPF6 in EC/EMC with 2 wt% VC).
  • Cell format: three-electrode laboratory cell or full cell, since the 0 V plating criterion is read against a reference electrode.
  • Loading: areal capacity of the electrode (Lu et al. discuss a 2 mAh/cm² electrode) and current density (Chen et al. report 10 mA/cm² as about 4.13C in their cells).
  • Temperature during charge, and the state-of-charge window or voltage cut-off used.
  • Whether capacity is quoted per gram of graphite or per gram of the whole electrode, given that 372 mAh/g refers to the active material.

The data table below collects the figures from these sources in one place, with the unit and the study or report each value comes from.

Sources

Data: Graphite anode figures: capacity, plating thresholds and US supply indicators

Selected quantitative figures for lithium-ion graphite anodes compiled from two peer-reviewed studies and the USGS Mineral Commodity Summaries 2026, with the unit and source for each value.

Period covered: 2023/2026.

Graphite anode figures: capacity, plating thresholds and US supply indicators
MeasureValueUnitSource
Theoretical capacity of LiC6372mAh/gChen et al. 2025
Charge before graphite potential reaches 0 V at -20 C412mAh/gChen et al. 2025
Charge before graphite potential reaches 0 V at -30 C160mAh/gChen et al. 2025
Charge before graphite potential reaches 0 V at -40 C106mAh/gChen et al. 2025
Modelled capacity loss, 1C charge to 100% SOC17%Lu et al. 2023
Modelled capacity loss, 1C with 75% SOC cut-off1.3%Lu et al. 2023
Modelled capacity loss, 1C with 65% SOC cut-off0.2%Lu et al. 2023
US net import reliance, natural graphite, 2025100%USGS MCS 2026
China share of world natural graphite mine production, 2025 (est.)82%USGS MCS 2026
US imports of graphite battery anode material, Jan-Aug 202543400tonnesUSGS MCS 2026
US imports of graphite battery anode material, Jan-Aug 202428100tonnesUSGS MCS 2026

Sources

Compiled by CASRAI from the sources above. Free to reuse under CC BY 4.0 with attribution.

Follow CASRAI

Research-administration guidance, standards updates and independent tool reviews.

Ask CASRAI · full access

Ask about Graphite Anode in Lithium-Ion Cells: How Lithium Fits Between the Layers

Full access: large monthly usage, up to 10 source passages behind each answer, and MCP and API access for Claude Code, Codex and other CLIs. Cancel any time.

An AI assistant for research: funder rules, compliance, methods and publishing. It links the sources behind its answers and labels answers that come from a web search.

Answers draw on CASRAI's guides and dictionary plus the federal and funder documents we index: Federal Register, Grants.gov, Regulations.gov and UKRI.

Works on this site and inside Claude, Cursor and the AI tools you already use.

Everything CASRAI publishes — this page, the dictionary, the guides and the news — stays open to read, with no account and no card.

Referenced across the research world

University of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logoUniversity of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logo
  • University of Cambridge logo
  • Columbia University logo
  • Crossref logo
  • University of Edinburgh logo
  • Harvard University logo
  • University of Oxford logo
  • Princeton University logo
  • Stanford School of Medicine logo
  • University College London logo
  • ORCID logo

View CASRAI adoption →