Written and maintained by CASRAI Editorial Board
Published
On this page
Short answer
A Pourbaix diagram (potential-pH or E-pH diagram) is a thermodynamic phase map plotting equilibrium states of an element in aqueous solution against electrochemical potential and pH. It identifies whether a metal under specific conditions remains thermodynamically immune, corrodes into soluble ions, or passivates by forming an insoluble protective oxide or hydroxide film.
Definition and scope
Formulated by Marcel Pourbaix in his 1966 Atlas of Electrochemical Equilibria in Aqueous Solutions, a Pourbaix diagram provides a thermodynamic map of aqueous chemical and electrochemical equilibria at 25°C and 1 atm. Under ASTM G3-14(2019) (Standard Practice for Conventions Applicable to Electrochemical Measurements in Corrosion Testing), potential-pH diagrams provide the standard thermodynamic baseline for evaluating corrosion potentials and polarization behavior. Researchers comparing thermodynamic theory with chemical synthesis often examine cross-disciplinary frameworks in materials science vs chemistry.
The diagram maps three primary thermodynamic domains:
- Immunity: The pure elemental metal is thermodynamically stable against oxidation; cathodic protection maintains metals in this domain where spontaneous dissolution cannot occur.
- Corrosion: Soluble ionic species (such as Fe²⁺ or HFeO₂⁻) represent the stable phase; active dissolution occurs where aqueous ion activity exceeds 10⁻⁶ mol/L (10⁻⁶ M).
- Passivation: Insoluble oxides or hydroxides (such as Fe₂O₃) form a coherent surface film that physically shields the substrate, drastically suppressing dissolution rates.
How it works or how it is used in practice
A Pourbaix diagram plots electrochemical potential (E, in volts vs. SHE) on the vertical Y-axis and pH on the horizontal X-axis. Under ASTM G3-14(2019) and the IUPAC Stockholm convention (1953), potentials follow the sign-invariant convention, with noble (oxidizing) potentials upward and active (reducing) potentials downward. Potentials recorded against laboratory reference electrodes (SCE or Ag/AgCl) must be converted to the Standard Hydrogen Electrode (SHE, 0.000 V) using high-impedance instruments such as an electrometer.
Phase boundary lines reflect three distinct reaction classes:
- Horizontal boundaries: Pure electron-transfer (redox) reactions independent of pH (e.g., Fe³⁺ + e⁻ ⇌ Fe²⁺).
- Vertical boundaries: Pure acid-base or precipitation equilibria independent of potential (e.g., Fe³⁺ + 3H₂O ⇌ Fe(OH)₃ + 3H⁺).
- Sloped boundaries: Coupled reactions involving both electrons and protons (e.g., 2Fe + 3H₂O ⇌ Fe₂O₃ + 6H⁺ + 6e⁻), exhibiting a theoretical Nernstian slope of -(0.0591 × m / n) V per pH unit at 298.15 K.
Two universal dashed lines define the thermodynamic stability domain of liquid water:
- Line (a) (Hydrogen Evolution): 2H⁺ + 2e⁻ ⇌ H₂(g), defined at 1 atm by E = -0.0591 × pH (V vs. SHE). Potentials below Line (a) reduce water to hydrogen gas.
- Line (b) (Oxygen Evolution): 2H₂O ⇌ O₂(g) + 4H⁺ + 4e⁻, defined at 1 atm by E = 1.229 – 0.0591 × pH (V vs. SHE). Potentials above Line (b) oxidize water to oxygen gas.
Liquid water is thermodynamically stable exclusively between Line (a) and Line (b).
Types or related concepts
Modern research utilizes both experimental binary diagrams and computational multi-element phase diagrams cataloged in computational materials data repositories.
| System / Metal | Immunity Regime (V vs. SHE) | Dominant Passive Film | Corrosion Vulnerability | Primary Application |
|---|---|---|---|---|
| Pure Iron (Fe-H₂O) | E < -0.44 V (pH 0); E < -0.85 V (pH 14) | Fe₃O₄, Fe₂O₃ (neutral/alkaline) | Acidic dissolution (Fe²⁺); caustic attack (HFeO₂⁻, pH > 13) | Structural steel, cathodic protection |
| Titanium (Ti-H₂O) | E < -1.63 V (below Line a) | TiO₂ (rutile/anatase, pH -2 to 16) | Hot concentrated non-oxidizing acids | Chemical vessels, biomedical implants |
| Copper (Cu-H₂O) | E < +0.34 V (pH 0, noble immunity) | Cu₂O, CuO (pH 7 to 13) | Acidic oxidizing media; cuprates at pH > 13 | Potable plumbing, marine piping |
| Zinc (Zn-H₂O) | E < -0.76 V (pH 0); E < -1.25 V (pH 14) | ZnO, Zn(OH)₂ (pH 8.5 to 11.0) | Amphoteric: dissolves in acids and strong bases | Galvanized coatings, battery anodes |
| Gold (Au-H₂O) | Immune across full water stability window | Au₂O₃ (anodic overpotentials above Line b) | Requires complexing ligands (cyanide, aqua regia) | Electronic interconnects, reference electrodes |
Where it matters for labs, clinics or supply decisions
Pourbaix diagrams guide alloy selection, experimental design, and corrosion testing protocols:
- Electrolyte Purity: Trace halides (Cl⁻) induce localized pitting breakdown without shifting thermodynamic oxide lines; labs prepare testing electrolytes using verified laboratory water purification systems.
- pH Stabilization: Electrochemical reactions consume or generate protons at electrode interfaces; researchers deploy standardized buffer solutions to maintain constant pH coordinates.
- Aeration Control: Dissolved oxygen elevates corrosion potentials toward Line (b); deaeration with high-purity argon shifts potentials toward Line (a).
- Computational Materials Genomics: Pymatgen and Materials Project tools compute ternary and quaternary Pourbaix diagrams combining DFT solid-phase energies with NIST-JANAF thermochemical aqueous datasets for multi-principal element alloys.
Common misunderstandings
Key misconceptions when applying Pourbaix diagrams include:
- Thermodynamics versus Kinetics: Pourbaix diagrams indicate only equilibrium stability (ΔG < 0), not corrosion rates. A metal in a corrosion zone may dissolve imperceptibly slowly, while a passive film may suffer rapid pitting if defective.
- Assuming Passivation Guarantees Protection: A thermodynamically stable oxide protects the substrate only if it is dense, adherent, and continuous. Non-adherent or porous oxides permit continuous corrosion.
- Temperature and Pressure Invariance: Standard diagrams assume 25°C and 1 atm. High-temperature systems (e.g., autoclaves at 300°C) experience severe contraction of the water stability zone and shifted phase boundaries.
- Fixed Ion Activity: Standard boundaries assume an aqueous ionic activity of 10⁻⁶ M. Altering concentration shifts dissolution boundaries by 59.1/n mV per decade of activity.
Frequently asked questions
What are the axes of a Pourbaix diagram?
The vertical Y-axis measures electrochemical potential (E in volts vs. SHE), while the horizontal X-axis measures electrolyte pH (typically -2 to 16).
What do the dashed lines signify on a Pourbaix diagram?
They represent the stability boundaries of water at 25°C and 1 atm: Line (a) denotes hydrogen evolution (E = -0.0591 × pH), and Line (b) denotes oxygen evolution (E = 1.229 – 0.0591 × pH). Liquid water is stable between them.
What is the difference between immunity and passivity?
Immunity signifies that the elemental metal is thermodynamically stable against oxidation. Passivity means the metal oxidizes to form an insoluble solid oxide film that impedes further active dissolution.
How does ASTM G3 relate to Pourbaix diagrams?
ASTM G3-14(2019) standardizes the Stockholm sign invariant convention, plotting noble (positive) potentials upward on the vertical axis, ensuring experimental polarization data directly match Pourbaix diagram axes.
Sources
- ASTM International. ASTM G3-14(2019): Standard Practice for Conventions Applicable to Electrochemical Measurements in Corrosion Testing. West Conshohocken, PA: ASTM International; 2019. Available from: https://www.astm.org/g0003-14r19.html (Accessed November 11, 2026).
- Pourbaix M. Atlas of Electrochemical Equilibria in Aqueous Solutions. 2nd English ed. Houston, TX: National Association of Corrosion Engineers (NACE International) / CEBELCOR; 1974. Available from: https://www.worldcat.org/title/atlas-of-electrochemical-equilibria-in-aqueous-solutions/oclc/1044437 (Accessed November 11, 2026).
- International Union of Pure and Applied Chemistry (IUPAC). Standard Electrode Potential. Compendium of Chemical Terminology (Gold Book). Research Triangle Park, NC: IUPAC; 2014. Available from: https://goldbook.iupac.org/terms/view/S05912 (Accessed November 11, 2026).
- Materials Project. Pourbaix Diagram Analysis and Documentation. Lawrence Berkeley National Laboratory; 2026. Available from: https://materialsproject.org/docs/analysis/pourbaix_diagram (Accessed November 11, 2026).
- Persson KA, Waldwick B, Lazic P, Ceder G. Prediction of solid-aqueous equilibria from first principles of solids and aqueous species. Physical Review B. 2012;85(23):235438. Available from: https://journals.aps.org/prb/abstract/10.1103/PhysRevB.85.235438 (Accessed November 11, 2026).