ASTM F2063 is the ASTM International specification for wrought nickel-titanium (nitinol) shape memory alloys used to make medical devices and surgical implants. It sets chemical, physical, mechanical and metallurgical requirements for the raw mill product (bar, plate, coil and tubing) containing nominally 54.5 % to 57.0 % nickel by weight. It does not describe a finished device, and it is paired in practice with other ASTM test methods that FDA names in its nitinol guidance.
This page describes products and general use; it is not medical advice.
Short answer: what ASTM F2063 is and is not
The current designation on the ASTM store page is F2063-26, listed as active and last updated 9 June 2026 (page read 2026-11-24); superseded editions listed there include F2063-18, -12, -05 and -00. Its formal title is “Standard Specification for Wrought Nickel-Titanium Shape Memory Alloys for Medical Devices and Surgical Implants” and it sits with ASTM Committee F04 on medical and surgical materials and devices, subcommittee F04.12. The standard is copyrighted, so this page paraphrases its scope and does not reproduce its tables or numerical limits; anyone who needs the limits must work from the licensed standard itself.
Three points cause most of the confusion. First, F2063 is a material specification: it covers mill product, not the final shape, surface finish or properties of a device. Second, it is a specification, not a performance test: transformation temperature, fatigue and corrosion behaviour of a finished device are judged with other methods. Third, conformity of the raw material does not by itself show that a finished nitinol device performs as intended.
Definition and scope
Nitinol is, in FDA’s words, “a nearly equiatomic metal alloy of nickel and titanium”. Its behaviour comes from reversible transformations between austenite and martensite phases. When the transformation is driven by temperature the behaviour is called shape memory; when it is driven by stress it is called pseudoelasticity (also called superelasticity). FDA notes that these properties let nitinol withstand greater reversible deformation without plastic deformation than stainless steel, titanium or cobalt-chrome alloys (FDA guidance, read 2026-11-24).
What the specification covers
- Alloy: wrought nickel-titanium containing nominally 54.5 % to 57.0 % nickel by weight, made from nickel and titanium with no other intentional alloy additions.
- Product forms: bar, flat-rolled product (plate), coil and tubing. The ASTM page states that finished nickel-titanium tube is covered by a separate standard, F2633.
- Mill size range: the scope describes mill product from 5.50 mm to 94.0 mm (0.218 in. to 3.70 in.) in diameter or thickness, and states that mill product is not intended to have the final shape, surface finish or properties of the device.
- Melting and supply condition: ingot is vacuum or inert-atmosphere melted to control cleanliness and chemistry; material is supplied hot or cold finished, annealed or heat treated.
- Surface condition: may be oxidized, descaled, pickled, blasted, machined, ground, mechanically polished or electropolished.
How conformity is checked
The ASTM abstract names the analytical routes without prescribing one method for every element: major elements by plasma spectrometry, atomic absorption, ICP, X-ray spectrometry, glow discharge mass spectrometry or an equivalent; carbon by combustion; hydrogen by inert gas fusion or vacuum hot extraction; nitrogen and oxygen by inert gas fusion. It also states a limit of chemical analysis that matters for the physical side of the standard: nickel and titanium contents cannot be measured precisely enough to guarantee shape memory or superelastic properties, so calorimetry or an equivalent thermomechanical test must be used to assure the alloy formulation in terms of transformation temperature. Tensile strength and elongation are determined on samples after annealing.
How ASTM F2063 is used in practice: the FDA submission view
FDA’s guidance “Technical Considerations for Non-Clinical Assessment of Medical Devices Containing Nitinol” (nonbinding; docket FDA-2019-D-1261; issued 9 July 2021 on the FDA page) is the clearest public statement of how F2063 fits into a premarket submission. In its Material Composition section FDA says that if the nitinol conforms to a recognized consensus standard, that information should be included in the submission, giving ASTM F2063 as the example. If the nitinol does not conform, FDA recommends providing the composition and a description of its specific properties. The guidance uses “should” to mean a recommendation, not a requirement.
The same guidance shows why F2063 alone is not enough. Its recommendations are written around the final finished device, including sterilisation, and apply most fully to prolonged-exposure and permanent-contact devices (the guidance follows ISO 10993-1 duration definitions: limited exposure up to 24 hours, prolonged exposure more than 24 hours up to 30 days, permanent contact more than 30 days). For limited-exposure devices some of the information may not be warranted. The main expectations are:
- Manufacturing description. A high-level flow chart from raw material to final sterilisation, because heat treatments and surface processing can change behaviour. Thermal steps of specific interest are laser cutting, annealing and thermal shape setting; surface steps include honing, microblasting, pickling, polishing and passivation, which affect corrosion and nickel release.
- Stated behaviour. The submission should say whether pseudoelastic or shape memory behaviour is used, or that neither is.
- Transformation temperatures on the finished form. Measured on the final finished form including sterilisation, using samples from a minimum of three production lots where possible, because transformation temperatures are sensitive to small process variations. For pseudoelastic use FDA recommends the austenite finish temperature (Af), the R-phase finish temperature (R′f) where an R-phase is present, or body-temperature mechanical data meeting pre-specified acceptance criteria; for shape memory use it also asks for As, Ms and Mf.
- Mechanical testing at a clinically relevant temperature, with preconditioning for deformations the device sees before use (for example stent crimping) and temperature excursions such as sterilisation. FDA does not recommend fatigue testing of nitinol in air because results are sensitive to test frequency through heating; it suggests a clinically relevant liquid such as phosphate buffered saline, or a scientific justification for another environment.
- Corrosion. Pitting corrosion testing for prolonged-exposure and permanent-contact devices; nickel ion release characterisation if acceptance criteria are not met or the surface finish is not an established one with a good clinical history (FDA names electropolishing, chemical etch and mechanical polishing as examples). Corrosion testing is generally not warranted for limited-contact devices, with exceptions such as an electrically active component or a dissimilar metal couple.
How FDA’s expectations change with duration of contact
The guidance scales its recommendations to how long the device is in contact with the body, using the ISO 10993-1 categories. The table summarises what the guidance says for each category; it is not a substitute for the guidance or for device-specific advice.
| Contact category (FDA, citing ISO 10993-1) | Definition in the guidance | General information and mechanical data | Corrosion testing |
|---|---|---|---|
| Limited exposure | Cumulative use or contact up to 24 hours | Some of the information may not be warranted; for example, functional testing of passive cardiac guidewires may be sufficient | Generally not warranted, but may be requested for an electrically active component, a dissimilar metal couple or a degradable metal or polymer |
| Prolonged exposure | Likely to exceed 24 hours but not 30 days | Full set of recommended general information provided | Pitting corrosion testing recommended |
| Permanent contact | Exceeds 30 days | Full set of recommended general information provided | Pitting corrosion testing recommended; nickel ion release characterised if criteria are not met or the finish is not an established one |
For devices that rely on computational stress and strain analysis, the guidance adds that nitinol’s constitutive behaviour differs substantially from conventional metals, that the material model parameters should be documented and justified, and that ASTM F2516 is a source for those parameters using specimens representative of the final device, including its heat treatment and surface processing.
Companion ASTM standards FDA names alongside F2063
The data table below maps each ASTM designation that appears in the FDA guidance (or on the F2063 page) to the role FDA or ASTM gives it. It is compiled from those two sources and is the quickest way to see where F2063 stops and the finished-device methods begin. One detail worth keeping from the guidance: FDA states that F2004 (thermal analysis) and F2082 (bend and free recovery) “do not necessarily measure the same Af temperature” for a given material or device, and for load-bearing devices it recommends F2082, modified to the strains the device will experience in its final form, because that method incorporates deformation.
Readers working on specific nitinol products can see how the material fits a device context in these CASRAI guides: orthodontic archwires, over-the-scope clips and ureteral stone retrieval baskets, all of which can be nitinol devices.
Where it matters for labs, quality teams and supply decisions
Because the standard is a material specification, the practical questions for a quality or compliance team are about what each document in the chain can and cannot demonstrate:
- Incoming material records. A statement that mill stock conforms to F2063 is evidence about composition and mill-product requirements. FDA asks that conformity to a recognized consensus standard be stated in the submission, so the record is something a submission can cite.
- Process control. Because FDA ties transformation temperature to the final finished form after sterilisation, a lab testing finished devices is generating different evidence from the material supplier’s certificate. FDA also asks for three production lots where possible.
- Test method selection. A transformation temperature reported by F2004 and one reported by F2082 should not be compared as if they were the same measurement. Reports should name the method.
- Quality system context. Device makers that source nitinol typically operate under a quality management system; see the CASRAI explainer on ISO 13485 and the guide on what makes a Class II medical device. FDA’s guidance itself refers readers to its 510(k) change guidance for modified devices.
This page does not state whether FDA has formally recognised a particular edition of F2063 under its consensus-standards programme; the FDA recognized-standards database is the place to check that for a given submission.
Common misunderstandings
“F2063 certifies the device”
It does not. The ASTM scope says mill product is not intended to have the final shape, surface finish or properties of a device, and FDA’s guidance asks for transformation temperatures, mechanical data and corrosion results on the final finished form.
“F2063 covers finished nitinol tubing”
The ASTM page assigns finished nickel-titanium tube to F2633. F2063 covers bar, plate, coil and tubing as mill product.
“A composition match guarantees superelasticity”
The F2063 abstract itself says nickel and titanium contents cannot be measured to the precision required to guarantee shape memory or superelastic properties, which is why a transformation-temperature test is required as well.
“Any Af result is interchangeable”
FDA cautions that F2004 and F2082 do not necessarily give the same Af for the same material or device, and that nitinol transformation temperatures vary with small changes in heat treatment.
“The FDA guidance is a rulebook”
The guidance is nonbinding. FDA uses “should” to mean something suggested or recommended, and an alternative approach may be used if it satisfies the requirements of the applicable statutes and regulations.
Sources
- ASTM International: F2063-26 Standard Specification for Wrought Nickel-Titanium Shape Memory Alloys for Medical Devices and Surgical Implants, checked 2026-11-24
- U.S. Food and Drug Administration: Technical Considerations for Non-Clinical Assessment of Medical Devices Containing Nitinol, checked 2026-11-24
- U.S. Food and Drug Administration: Technical Considerations for Non-Clinical Assessment of Medical Devices Containing Nitinol (guidance PDF), checked 2026-11-24
- ASTM International: Work item WK90888 (F2063 revision), checked 2026-11-24
Data: ASTM standards named with nitinol F2063 and the role each plays
Original compilation of ASTM designations that appear on the ASTM F2063-26 store page or in FDA's nitinol non-clinical guidance, with the property each addresses and the role the source gives it. Compiled 2026-11-24 from those two sources only; standard text and limits are not reproduced.
| ASTM designation | Subject | Role given by the source | Source |
|---|---|---|---|
| F2063 | Wrought nickel-titanium shape memory alloys for medical devices and surgical implants | Material specification for mill product (bar, plate, coil, tubing); named by FDA as an example consensus standard for composition | ASTM store page; FDA guidance |
| F2005 | Terminology for nickel-titanium shape memory alloys | Defines nitinol terminology; cited by FDA for its definitions | FDA guidance |
| F2633 | Finished nickel-titanium tube | ASTM states finished NiTi tube is covered here rather than by F2063 | ASTM store page |
| F2004 | Transformation temperature of NiTi alloys by thermal analysis | Recommended method for transformation temperatures; may not give the same Af as F2082 | FDA guidance |
| F2082 | Transformation temperature by bend and free recovery | Recommended for load-bearing devices when modified to the device's expected strains | FDA guidance |
| F2516 | Tension testing of nickel-titanium superelastic materials | Source of material-model parameters for computational analyses | FDA guidance |
| F2477 | In vitro pulsatile durability testing of vascular stents | Cited as an example of pressure control with displacement monitoring in radial pulsatile fatigue testing | FDA guidance |
| F2129 | Cyclic potentiodynamic polarization for corrosion susceptibility of small implant devices | Recommended method for pitting corrosion testing after simulated assembly and implantation; has no acceptance criterion of its own | FDA guidance |
| F3306 | Ion release evaluation of medical implants | Recommended method for nickel ion release testing when corrosion criteria are not met | FDA guidance |
Sources
- ASTM International: F2063-26 store page (accessed 2026-11-24)
- FDA: Technical Considerations for Non-Clinical Assessment of Medical Devices Containing Nitinol (accessed 2026-11-24)