Skip to main content
v2026.11,986 entries · CC-BY 4.0

Fly Ash Concrete: Class F vs Class C, ASTM C618 Limits and Lab Checks

What fly ash concrete is, how Class F and Class C differ, ASTM C618 and AASHTO M 295 limits, and the QC checks a lab runs.

Written and maintained by CASRAI Editorial Board

Published

On this page

Fly ash concrete is concrete in which part of the portland cement is replaced, or supplemented, by fly ash, the fine mineral residue left after pulverised coal is burned. The fly ash reacts with the calcium hydroxide that cement produces and adds binder, so the mix usually gains strength more slowly at first but can match or exceed cement-only concrete later. Specifiers classify the ash as Class F or Class C under ASTM C618.

Short answer

In North American practice fly ash is batched at the ready-mix plant as a partial replacement for portland cement. FHWA guidance reports typical dosages of 15 to 25 percent of the cementitious material by weight for Class F ash and 20 to 35 percent for Class C ash. Those percentages are starting points: they have to be confirmed with trial mixes made from the actual ash and the actual cement.

For a laboratory or quality-control team the useful questions are which class of ash the specification calls for, which ASTM C618 or AASHTO M 295 limits apply, how setting time and air content change, and which durability tests the particular ash needs. This page walks through each of them using FHWA and EPA documents.

Definition and scope

FHWA Materials Note 51 describes fly ash as the finely divided residue from the combustion of ground or powdered coal, with properties that depend on the coal and on how the power plant is operated. ASTM C618 covers three designations: Class N (natural pozzolans), Class F and Class C (coal fly ashes). This page deals with the two coal fly ash classes.

A pozzolan is a siliceous or aluminous material that has little binding value alone but, in fine form and in the presence of moisture, reacts with calcium hydroxide to form compounds with binding properties. The FHWA tech brief on supplementary cementitious materials explains that portland cement hydration releases calcium hydroxide (CH), and that the pozzolanic reaction consumes this CH and produces additional calcium silicate hydrate (CSH). That reaction is the underlying reason supplementary cementitious materials (SCMs) contribute to durability.

Fly ash is one SCM among several. Slag cement and silica fume are the other common ones, and they behave differently: the same FHWA brief notes, for instance, that slag cement needs replacement levels above 50 percent of the cement to match the alkali-silica reaction (ASR) mitigation of Class F fly ash. Natural pozzolans (Class N) and the blended cements discussed below are related but separate topics.

How fly ash works in concrete

Fly ash can be added directly into ready-mixed concrete at the batch plant as a partial replacement for, or an addition to, portland cement. It can also be interground with cement clinker or blended with portland cement to make blended cements. FHWA states that coal fly ash has been used in portland cement concrete as a mineral admixture for nearly 60 years (as of its 1997 guideline).

The mix design approach FHWA describes is to start from an all-portland-cement mix, remove some of the cement, and add fly ash to compensate. Class C ash is usually substituted at a 1:1 ratio by mass. Class F ash may also be substituted 1:1 but is sometimes specified at 1.25:1 and occasionally at 1.5:1. Some states require ash to be added to certain mixes with no reduction in cement content. FHWA also reports that ACI suggests making a trial mix for each 5 percent increment of replacement.

What changes in the fresh and hardened concrete

  • Workability and bleeding. FHWA lists improved workability and finishing among the benefits of properly proportioned fly ash mixes.
  • Time of set. Materials Note 51 says both classes extend the set time by 2 to 4 hours, varying from source to source, and that accelerators can be used to control it. The 1997 guideline adds that finishing of Class F mixes may have to be delayed by 1 to 2 hours depending on temperature, and that delays are more pronounced in cool or cold weather.
  • Heat of hydration. Lower for Class C and significantly lower for Class F in the FHWA tech brief.
  • Permeability. The tech brief rates fly ash as reducing permeability, the property behind much of the durability case. See the CASRAI guide on concrete durability, exposure classes and w/cm limits for how permeability enters ACI 318 requirements.
  • Air entrainment. Carbon in the ash, indicated by loss on ignition, reduces the air entrained for a given dose of air-entraining agent and absorbs water, so the admixture dose and water demand may need adjusting.

Class F and Class C fly ash compared

ASTM C618 classifies coal fly ash by composition. The FHWA tech brief reports that Class F requires a sum of the oxides (SiO2 + Al2O3 + Fe2O3) of 70 percent or more, and Class C 50 percent or more; Class F ash is pozzolanic, and Class C ash is predominantly hydraulic with some pozzolanic properties. FHWA’s 1997 guideline puts it in source terms: Class F is usually produced from anthracite or bituminous coal and Class C usually from lignite or subbituminous coal. Class F has little or no cementing value on its own, while Class C is self-cementing as well as pozzolanic.

The data table at the end of this page compares the two classes property by property using the FHWA documents. The specification limits that apply to either class are in the table below.

Item Limit Where stated
Maximum retained on 0.045 mm (No. 325) sieve, wet sieved 34 percent ASTM C618, as cited by FHWA
Minimum pozzolanic activity index with portland cement at 28 days (ASTM C311) 75 percent of the control mix strength ASTM C618, as cited by FHWA
Maximum loss on ignition, Classes C and F 6 percent ASTM C618
Maximum loss on ignition, Classes C and F 5 percent AASHTO M 295
Maximum loss on ignition in practice 5 percent for most state agencies; 3 to 4 percent for many state transportation departments FHWA Materials Note 51; FHWA-RD-97-148
Maximum moisture 3.0 percent ASTM C618, as cited by FHWA

The loss on ignition row is the one that most often causes disagreement between a purchase specification and a test report. FHWA Materials Note 51 explains that most state highway agencies specify fly ash by ASTM C618 except for the LOI requirement, where most specify a maximum of 5 percent, and the 1997 guideline notes that carbon contents above roughly 3 to 4 percent have an adverse effect on air entrainment. A lab reading an LOI of 5.5 percent therefore gets a pass against ASTM C618 and a fail against AASHTO M 295 and most agency specifications; the governing document is the project specification, not the generic standard.

Where it matters for labs and quality control

FHWA recommends that fly ash for concrete be as consistent and uniform as possible and be monitored under a QA/QC program that follows ASTM C311. That standard sets sampling methods and test frequencies for fineness, LOI, specific gravity and pozzolanic activity, so that the consistency of an ash source can be certified. Because the ash changes with the coal and plant operation, a lot-to-lot check is part of the control, not an extra.

A checklist built from the FHWA guidance

  1. Confirm the class and the governing specification (ASTM C618, AASHTO M 295 or the agency’s own) and its LOI limit before testing, since the limits differ as shown above.
  2. Record fineness (percent retained on the 0.045 mm sieve), LOI, specific gravity and pozzolanic activity index per ASTM C311 for each source, and watch uniformity between lots. Materials Note 51 mentions an optional uniformity requirement limiting variation in air-entraining agent demand to 20 percent.
  3. Make trial mixes at the replacement levels under consideration, stepping through the range in 5 percent increments as ACI suggests, and compare setting time and strength gain with the cement-only control.
  4. Check fresh air content on every trial batch, because carbon in the ash changes air-entraining agent demand. The CASRAI pages on ASTM C173 volumetric air content and ASTM C138 unit weight, yield and air content cover the two common fresh-concrete tests.
  5. Where alkali-silica reaction is a risk, verify the particular ash and aggregate combination by test rather than assuming a class-wide result. The FHWA brief points to ASTM C1567 and, in some cases, ASTM C1293; the related accelerated mortar-bar method is explained in the CASRAI guide to ASTM C1260.
  6. Plan for cold weather and curing: FHWA warns that cold temperatures slow strength gain, that Class F is the greater concern, and that some states set a cut-off date after which ash is not permitted until the following spring.
  7. Do not add ash on top of a blended cement that already contains pozzolan (see types below).

Sulfate resistance and ASR

FHWA’s 1997 guideline states that Class F ash generally improves sulfate resistance, while a Class C ash has to be tested individually because its behavior varies. For ASR the picture is similar: a Class F ash, being pozzolanic, is described as an excellent mitigation tool, but because ash properties vary, the mitigation potential should be verified. For Class C the tech brief says relatively higher replacement levels are needed, for example 35 to 45 percent, and its Table 1 describes Class C ASR mitigation as effective only at high replacements. The 1997 guideline suggests ASTM C441 for testing Class C ashes with field materials.

Environmental and supply context

EPA treats fly ash used in concrete as an encapsulated beneficial use of coal combustion residuals. The agency’s evaluation concluded that this use is appropriate because environmental releases are comparable to or lower than those from analogous non-CCR products or are at or below relevant benchmarks. EPA cites an American Coal Ash Association survey estimate that about 15 million tons of coal combustion residuals went into concrete, concrete products and grout in 2024, with about 63.6 million tons of CCR generated by coal-fired utilities that year. The supply of ash depends on the coal fleet, which is one reason sources and their quality vary.

ASTM C595 defines two blended cements that already contain fly ash or another pozzolan. FHWA describes Type IP (portland-pozzolan cement) as containing 15 to 40 percent pozzolan and Type I-PM (pozzolan-modified portland cement) as containing less than 15 percent. When one of these is used, FHWA recommends that no further fly ash be added to the mix, and the blended cement can be used in mix design in essentially the same way as a Type I portland cement. Materials Note 51 adds that most states specify limits on the pozzolan content of Type IP cement, between 15 and 25 percent.

Common misunderstandings

  • “Fly ash concrete is weaker.” Early strength of Class F mixes is lower, and FHWA’s 1997 guideline says strength can take 60 to 90 days to catch up to and exceed cement-only concrete, while the tech brief shows 28 to 56 day strength as the same or higher for both classes. The age at which strength is specified therefore matters.
  • “Class C and Class F are interchangeable.” The two differ in set time effects, early strength, heat, ASR mitigation and sulfate behavior; the dosage ranges also differ.
  • “Any fly ash will do.” FHWA’s 1997 guideline said only a minority of the coal fly ash then produced was potentially suitable for concrete; ash has to meet the specification and be consistent from lot to lot.
  • “The ASTM limit is the only limit.” Agency LOI limits of 3 to 5 percent are stricter than the ASTM C618 maximum of 6 percent.
  • “Fly ash concrete is a different product that needs separate handling.” FHWA states that placement and handling are in most respects similar to normal concrete, with allowances for slower setting and finishing.

Note that the 1997 FHWA guideline is archived and several of its figures date from that time. The 2016 tech brief and the later Materials Note are consistent with it on the points cited here.

Frequently asked questions

What is fly ash concrete made of?

It is concrete made with portland cement, water, aggregates and fly ash, where the ash replaces or supplements part of the cement. FHWA gives typical ash contents of 15 to 25 percent (Class F) and 20 to 35 percent (Class C) of the total cementitious material by weight.

What is the difference between Class F and Class C fly ash?

Under ASTM C618, Class F is the more pozzolanic ash (oxide sum of 70 percent or more) and Class C is self-cementing as well as pozzolanic (oxide sum of 50 percent or more). Class C usually gives higher early strength; Class F is the stronger ASR mitigator.

Does fly ash make concrete set slower?

Generally yes. FHWA reports that both classes extend set time by 2 to 4 hours, varying by source, and that accelerators can control it. Some Class C ashes have little effect or even shorten setting time.

What loss on ignition is allowed in fly ash for concrete?

ASTM C618 allows a maximum of 6 percent and AASHTO M 295 a maximum of 5 percent. Many state transportation departments specify 3 to 4 percent, because higher carbon content hurts air entrainment.

Is fly ash concrete safe for the environment?

EPA’s evaluation concluded that fly ash used as a direct substitute for portland cement in concrete is an appropriate encapsulated beneficial use, because environmental releases are comparable to or lower than those from analogous products made without coal combustion residuals.

Sources

Data: Class C versus Class F fly ash: effects on concrete properties and dosage

Property-by-property comparison of Class C and Class F coal fly ash substituted for portland cement, compiled from the FHWA supplementary cementitious materials tech brief (2016) and the FHWA coal fly ash user guideline (1997) and Materials Note 51.

Period covered: 1997/2016. Coverage: United States.

Class C versus Class F fly ash: effects on concrete properties and dosage
PropertyClass C fly ashClass F fly ashSource
Sum of oxides (SiO2 + Al2O3 + Fe2O3), minimum50% or more; predominantly hydraulic with some pozzolanic properties70% or more; pozzolanicFHWA-HIF-16-001
Typical coal sourceUsually lignite or subbituminousUsually anthracite or bituminousFHWA-RD-97-148
Typical share of total cementitious material by weight20 to 35 percent15 to 25 percentFHWA-RD-97-148
Usual substitution ratio for removed cement1:11:1, sometimes 1.25:1 or 1.5:1FHWA-RD-97-148
Initial setDelayed (some sources have little effect)DelayedFHWA-HIF-16-001; FHWA-RD-97-148
Rate of strength gainSame or higherSlowerFHWA-HIF-16-001
Heat of hydrationLowerSignificantly lowerFHWA-HIF-16-001
Early strength (3-7 days)HigherLowerFHWA-HIF-16-001
Late strength (28-56 days)Same or higherSame or higherFHWA-HIF-16-001
ASR mitigationOnly at high replacements (e.g. 35 to 45 percent)Significant above the pessimum replacement levelFHWA-HIF-16-001
Sulfate resistanceMust be tested for each ashGenerally improvedFHWA-RD-97-148

Sources

Compiled by CASRAI from the sources above. Free to reuse under CC BY 4.0 with attribution.

Follow CASRAI

Research-administration guidance, standards updates and independent tool reviews.

Ask CASRAI · full access

Ask about Fly Ash Concrete: Class F vs Class C, ASTM C618 Limits and Lab Checks

Full access: large monthly usage, up to 10 source passages behind each answer, and MCP and API access for Claude Code, Codex and other CLIs. Cancel any time.

An AI assistant for research: funder rules, compliance, methods and publishing. It links the sources behind its answers and labels answers that come from a web search.

Answers draw on CASRAI's guides and dictionary plus the federal and funder documents we index: Federal Register, Grants.gov, Regulations.gov and UKRI.

Works on this site and inside Claude, Cursor and the AI tools you already use.

Everything CASRAI publishes — this page, the dictionary, the guides and the news — stays open to read, with no account and no card.

Referenced across the research world

University of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logoUniversity of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logo
  • University of Cambridge logo
  • Columbia University logo
  • Crossref logo
  • University of Edinburgh logo
  • Harvard University logo
  • University of Oxford logo
  • Princeton University logo
  • Stanford School of Medicine logo
  • University College London logo
  • ORCID logo

View CASRAI adoption →