Skip to main content
v2026.11,986 entries · CC-BY 4.0

Fractography: What It Is and How Fracture Surfaces Are Read

Fractography is the examination of fracture surfaces to find how a material failed. Learn the examination sequence, failure-mode features and handling rules.

Written and maintained by CASRAI Editorial Board

Published

On this page

Fractography is the examination and interpretation of fracture surfaces. Laboratories use it to work out why a material or component failed, how the failure happened and how the crack progressed, by reading features on the broken surface from a visual inspection up to scanning electron microscopy.

Definition and scope

Xometry’s materials resource describes fractography as the “examination and interpretation of fracture surfaces” and says it is used to determine what caused a material to fail, how the failure occurred and how it progressed. ASM International’s Metals Handbook, Volume 12: Fractography (1987) treats it more broadly: its articles cover fracture examination and interpretation, including electron and quantitative fractography, and the principal fracture modes, along with how loading history, environment and material quality change the way a fracture looks.

The scope is the fracture surface itself, not the whole failure investigation. A broken part is also sectioned, polished and etched so the microstructure can be examined, and surface analysis can be added to evaluate chemical composition and contamination. Fractography is the step that reads the surface the crack left behind. The same handbook extends the subject beyond metals: its supplemental illustrations show failed metal-matrix composites, resin-matrix composites, polymers and electronic materials.

How fractography is used in practice

PACE Technologies’ failure analysis guide orders the work from the coarsest view to the finest. Each stage answers a different question, which is why the order matters: the early, non-destructive stages must be finished before any cutting is done.

Stage What is done What it contributes
Visual and macroscopic examination Fracture appearance, initiation sites, deformation and corrosion are recorded and photographed. Stereo microscopes and cameras are the macroscopic tools. Where the crack started and what the overall surface looks like, before anything is touched or cut.
Cross-section (metallographic) examination Sections are cut perpendicular to the fracture surface, then mounted, ground, polished and etched. The microstructure is examined at the origin and in an unaffected area. Microstructure at the failure origin compared with undamaged material.
Scanning electron microscopy Fracture features are imaged at high resolution, propagation direction is determined and the features are correlated with the microstructure. Microscopic features such as dimples and striations that identify the fracture mode.

Xometry gives a complementary list of techniques: visual inspection, optical microscopy (“commonly” 10 times to 1,000 times), scanning electron microscopy, stereomicroscopy for three-dimensional observation of surface topography and crack paths, digital imaging to record and measure features, and surface analysis. The optical range matters because light microscopes have a resolution limit of their own, discussed in the guide to the optical microscopy resolution limit; the electron microscope takes over where that limit is reached, as compared in SEM versus TEM.

Reading features by failure mode

The data table below sets out what the two failure-analysis sources list for each mode. The patterns are described qualitatively; none of the sources used here gives a numeric threshold that separates one mode from another, so the table is a guide to what to look for, not a classification rule.

Ductile fracture

Ductile failure follows substantial plastic deformation and absorbs significant energy. PACE lists necking, reduction in cross-sectional area, cup-and-cone fracture surfaces and evidence of plastic deformation in the microstructure. At high magnification the surface is dimpled; Xometry attributes the dimples to microvoid growth and coalescence.

Brittle fracture

Brittle failure shows minimal plastic deformation and proceeds rapidly once the crack starts. PACE describes flat, featureless surfaces, cleavage facets in crystalline materials and river patterns; Xometry adds that brittle surfaces display cleavage facets or intergranular features.

Fatigue fracture

Fatigue develops under repeated cyclic loading, with the crack advancing in increments. PACE lists beach marks or striations, multiple crack initiation sites, progressive crack growth patterns and a final fast-fracture region. Beach marks are the macroscopic bands; striations are the microscopic ones.

Creep fracture

PACE lists grain boundary cavitation, elongated grains in the direction of stress, intergranular fracture surfaces and time-dependent deformation as the features that point to creep.

A worked example from the published literature: reading a fatigue surface

In a case study published in Advanced Materials and Processes in September 2019, Richard Ellsworth and Chris Spies of EDT Forensic Engineering and Consulting examined a fatigue fracture and showed how several surface features should and should not be interpreted. Their observations are a useful checklist of what an examiner is looking at.

  • Beach marks. The arcs on the smooth fatigue zone mark where cracking paused when the load dropped below a damaging level and resumed when it returned. The arcs grow larger as they move across the surface.
  • A rust-coloured arc. The authors treat a dark, rust-coloured arc as a visual sign of fatigue and note that rusting is typical of fatigue fractures of iron and steel parts. Fresh fracture surfaces on such parts sit exposed to the environment for a long time before final failure.
  • Shiny spots. These form where raised areas on the two mating fracture surfaces were flattened by repeated contact after the initial crack formed.
  • Staged SEM imaging. The shiny spots were visible at 50 times but did not give the full picture; at 250 times the flattening of the contacting areas was confirmed; at 1,000 times, aligned striations appeared on an unflattened, unaltered part of the surface.

The authors describe aligned microscopic striations as characteristic of fatigue fractures and note that striation spacing can indicate changes in loading during crack growth, with wider spacing implying higher load and narrower spacing lower load. The practical lesson is the sequence: the features that are easiest to see at low magnification can be altered after the crack formed, so the decisive evidence came from an area that had not been damaged by contact.

Handling the fracture surface in the laboratory

For laboratory staff the largest influence on a fractographic result is often what happens before the specimen reaches the microscope. PACE’s failure analysis guide gives these working rules:

  • Preserve fracture surfaces where possible.
  • Protect fracture surfaces from damage and contamination.
  • Store samples properly to prevent further degradation.
  • Document everything before destructive testing, photographing all relevant features during macroscopic examination.
  • Select samples from the failure origin and from unaffected areas.
  • Prepare cross-sections perpendicular to the fracture surface.
  • Maintain chain of custody for legal cases.

These rules follow from the case study above: because the surface keeps changing after fracture (rusting, rubbing of mating faces), a surface that is touched, cleaned or left unprotected can lose the evidence an examiner needs. The chain-of-custody rule is the same principle that governs other evidence handling, covered in the guide to chain of custody in forensic science. Where the failure involved a corrosive environment, the separate guide to stress corrosion cracking describes that mechanism.

Reference material: the ASM atlas

Interpreting a fracture surface is largely pattern recognition against known examples. The standard reference named in the sources is Metals Handbook, Volume 12: Fractography, published by the American Society for Metals in 1987. According to the OSTI record, the second half of the volume is an atlas of more than 1,300 fractographs, including ferrous and nonferrous alloy parts, accompanied by line drawings, graphs and photographs of fracture surfaces and microstructural features. The record is a catalogue description, so it tells a laboratory what the volume contains, not what it concludes.

Where it matters for labs

Fractography is relevant wherever a laboratory receives broken parts, test coupons or failed components and has to say how they broke. Three points from the sources apply directly to laboratory practice. First, the examination order is fixed by the need to document before destructive work, so the macroscopic record has to be complete before sectioning begins. Second, sampling at both the failure origin and an unaffected area gives the examiner a comparison, which is how features at the origin can be judged against normal microstructure. Third, a result that may be used in a legal case depends on a documented chain of custody, which has to be started when the specimen is received.

Common misunderstandings

  • Fractography is more than looking through a microscope. The sources describe it as the interpretation of fracture surfaces using several methods, from visual inspection and stereomicroscopy to SEM, with digital imaging and surface analysis as supporting techniques.
  • Colour and shine are not the whole story. A rust-coloured arc and shiny spots record what happened to the surface after cracking began. In the ASM case study the flattening was confirmed at higher magnification and the diagnostic striations were found on a part of the surface that had not been altered.
  • Striation spacing is not a load measurement. The authors say spacing can indicate a change in loading, wider implying higher load. That is a relative statement about how loading varied during crack growth.
  • The fracture modes are not metal-only categories. The ASM handbook’s supplement covers composites, polymers and electronic materials as well as metals.
  • The table of features is not a decision rule. The sources list typical features for each mode; they do not set numeric cut-offs, and a real specimen may show features of more than one mode.

Sources

Data: Fracture-surface features by failure mode

Compiled from three failure-analysis sources: PACE Technologies' failure analysis guide, Xometry's fractography resource and a 2019 ASM Advanced Materials & Processes fatigue case study. Each row lists the macroscopic or whole-specimen features and the microscopic features the sources associate with a failure mode. Qualitative descriptions only; no source gives numeric cut-offs.

Fracture-surface features by failure mode
Failure modeMacroscopic or specimen-level featuresMicroscopic fracture-surface featuresSources
DuctileNecking and reduction in cross-sectional area; cup-and-cone surface; plastic deformation in the microstructureDimpled appearance at high magnification, from microvoid growth and coalescencePACE Technologies; Xometry
BrittleFlat, featureless surface; minimal plastic deformation in surrounding materialCleavage facets in crystalline materials; river patterns; intergranular featuresPACE Technologies; Xometry
FatigueBeach marks (macroscopic bands); multiple crack initiation sites; progressive crack growth; final fast-fracture regionStriations (microscopic); aligned striations characteristic of fatiguePACE Technologies; Xometry; ASM Advanced Materials & Processes (2019)
CreepTime-dependent deformation; elongated grains in the direction of stressGrain boundary cavitation; intergranular fracture surfacePACE Technologies

Sources

Compiled by CASRAI from the sources above. Free to reuse under CC BY 4.0 with attribution.

Follow CASRAI

Research-administration guidance, standards updates and independent tool reviews.

Ask CASRAI · full access

Ask about Fractography: What It Is and How Fracture Surfaces Are Read

Full access: large monthly usage, up to 10 source passages behind each answer, and MCP and API access for Claude Code, Codex and other CLIs. Cancel any time.

An AI assistant for research: funder rules, compliance, methods and publishing. It links the sources behind its answers and labels answers that come from a web search.

Answers draw on CASRAI's guides and dictionary plus the federal and funder documents we index: Federal Register, Grants.gov, Regulations.gov and UKRI.

Works on this site and inside Claude, Cursor and the AI tools you already use.

Everything CASRAI publishes — this page, the dictionary, the guides and the news — stays open to read, with no account and no card.

Referenced across the research world

University of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logoUniversity of Cambridge logoColumbia University logoCrossref logoUniversity of Edinburgh logoHarvard University logoUniversity of Oxford logoPrinceton University logoStanford School of Medicine logoUniversity College London logoORCID logo
  • University of Cambridge logo
  • Columbia University logo
  • Crossref logo
  • University of Edinburgh logo
  • Harvard University logo
  • University of Oxford logo
  • Princeton University logo
  • Stanford School of Medicine logo
  • University College London logo
  • ORCID logo

View CASRAI adoption →