Written and maintained by CASRAI Editorial Board
Published
On this page
Pavement design is the engineering process of choosing the layers, materials and thicknesses of a road, airfield or parking surface so that it carries its forecast traffic safely and durably for a chosen design period. In US highway work the governing rule is a performance goal, not a method: 23 CFR 626.3 says pavement “shall be designed to accommodate current and predicted traffic needs in a safe, durable, and cost effective manner,” and each State Highway Agency selects the procedure it uses.
Short answer: what pavement design decides
A pavement design answers one question: what structure, built from which materials, will keep a surface in acceptable condition under the traffic, climate and soil it will actually meet? The design produces a layered structure and the material properties it relies on. It is then judged against predicted deterioration (cracking, rutting, faulting, roughness) or against an empirically derived load-carrying capacity, depending on the method.
This page is written for researchers, lab staff and materials-testing teams who supply the inputs to those designs. It explains where the US federal requirement comes from, how the long-standing empirical AASHTO 1993 approach differs from the mechanistic-empirical (M-E) approach, which inputs each method needs, and where laboratory and field testing feed in. It does not give thicknesses, layer recipes or design steps: those belong to the method your agency has adopted and to a licensed engineer.
Definition and scope of pavement design
Pavement design sits between traffic forecasting, geotechnical investigation and materials characterization. Three kinds of work feed it:
- Traffic. FHWA’s pavement design guidance treats the cumulative load carried over the design period as central to structural design. Estimates should rest on current vehicle classification and weight data and on expected truck growth, collected with statistically valid counting methods.
- Foundation. The same guidance calls a uniform, stiff, moisture- and frost-resistant foundation the most important factor in structural design.
- Materials. Layer stiffness and strength come from laboratory tests and, for existing pavements, from field deflection testing.
The scope covers new construction, reconstruction and rehabilitation. FHWA describes major rehabilitation design as four phases: project evaluation (condition, traffic, environment and materials, using pavement management data, coring and deflection testing), project analysis (comparing feasible alternatives on engineering and life-cycle cost), project design, and project implementation (documenting design intent in plans and specifications and feeding as-built and performance data back into the pavement management system).
Pavement design is distinct from geometric design. The AASHTO Green Book concerns the geometry of roads (alignment, sight distance, cross-section), not the structural design of the pavement layers. Airport pavements follow separate procedures; the FAA’s tool is covered in the guide to FAARFIELD.
How pavement design is done in practice: a rule, not a recipe
The federal requirement
FHWA’s pavement design page, formerly a non-regulatory supplement to 23 CFR Part 626 and last updated 23 September 2021, states that the regulation sets a performance goal and does not prescribe a design method. Each State Highway Agency (SHA) selects a procedure suited to its conditions: the AASHTO guide, or another method backed by past performance or research. FHWA field offices may periodically review an SHA’s design process by sampling enough projects to confirm that the process is followed and produces reasonable results. Where the process is acceptable and followed, FHWA states that routine pavement design reviews of individual projects will not be required. FHWA also encourages mechanistic design procedures.
The practical consequence for a researcher is that “the” pavement design method does not exist at the national level. A test result that is a required input in one agency’s procedure may be optional in another’s, so the first step in any materials-characterization project is to identify which procedure the agency commissioning the work actually uses.
The AASHTO 1993 empirical approach
The 1993 AASHTO guide relies on empirical equations derived from the AASHO Road Test of 1958 to 1960. FHWA’s description of that test is that it used a limited number of pavement sections at a single location, with traffic well below present-day levels. In the 1986 and 1993 editions the key roadbed-soil input for flexible pavements is resilient modulus (MR), which replaced the earlier soil support value. FHWA’s design guidance says the AASHTO guide strongly recommends that agencies acquire the equipment to measure MR, and that agencies converting MR from California Bearing Ratio or R-value should run correlation studies across soil types, moisture levels and densities. For rigid pavements the foundation input is a k-value.
Traffic enters as cumulative 18-kip equivalent single axle loads (ESALs). FHWA advises that forecasts cover at least two truck groups, vehicles up to four-axle combinations and vehicles with five or more axles, and that weigh-in-motion data are preferable to static scales, which are prone to avoidance.
The mechanistic-empirical approach
The M-E Pavement Design Guide was developed under NCHRP Project 1-37A and released in 2004 as a review version for agencies to test. FHWA describes it as a uniform basis for designing flexible, rigid and composite pavements, applicable to new, reconstructed and rehabilitated pavements, and intended to replace the 1993 guide. It analyzes traffic, climate, materials and the proposed structure, and uses numerical models to estimate damage accumulation over the service life. Outputs are predicted distress and smoothness, which can be compared with threshold values or with alternative designs. The guide also supports designs with special loadings such as multiple tires or axles, evaluation of design variability and reliability, and analysis of existing pavements to identify deficiencies.
The software implementation is AASHTOWare Pavement ME Design. FHWA’s LTPP calibration work (FHWA-HRT-17-104, 2018) used version 2.2, retained the software’s default 20-year design life, and calibrated the rutting models for new and overlaid flexible pavements so that calculated total rutting matched measured LTPP rutting. That study shows concretely what the inputs look like; the data table below compiles them.
Empirical versus mechanistic-empirical design: a side-by-side
| Aspect | AASHTO 1993 guide | M-E design (NCHRP 1-37A, Pavement ME) |
|---|---|---|
| Basis | Empirical equations from the AASHO Road Test, 1958 to 1960 | Numerical models of damage accumulation over service life, using data from across the US |
| Evidence base | Limited sections at one location; traffic well below today’s | Nationally calibrated distress models that States can use for design and analysis |
| Roadbed soil input (flexible) | Resilient modulus (MR), replacing soil support value | Material properties at hierarchical input levels; unbound-material resilient modulus treated as level 2 in the LTPP calibration |
| Pavement types | Flexible and rigid design procedures | Flexible, rigid and composite; new, reconstructed and rehabilitated |
| Output | Structure sized against a load-carrying criterion | Predicted distress and smoothness, compared with thresholds |
Reading note: the rows describe what FHWA’s documents state about each approach; they are not a ranking. FHWA describes the M-E guide as intended to replace the 1993 guide, while the pavement design page confirms that agencies remain free to choose the procedure they use.
Types of pavement and what the M-E models predict
The M-E guide treats three structure types, and the distresses it predicts differ by type:
- Flexible pavements: longitudinal cracking, alligator cracking, transverse cracking and rutting.
- Rigid pavements: faulting, cracking, and continuously reinforced concrete pavement (CRCP) punch-outs.
- Composite pavements: designed on the same uniform basis; smoothness is predicted alongside distress.
For researchers, this list is a useful map from a distress mode to the material properties that govern it. Rutting prediction depends on asphalt-layer and unbound-layer properties, which is why the LTPP calibration paid close attention to asphalt dynamic modulus and unbound resilient modulus. Reclaimed material is covered in the guide to recycled asphalt pavement.
Where pavement design matters for labs and research offices
Input levels and what a lab test buys
The M-E procedure grades inputs by hierarchy. In the FHWA-HRT-17-104 calibration, level 1 for the asphalt layer meant laboratory-measured binder, volumetric, dynamic modulus and creep compliance data wherever those were available. The dynamic modulus values in that study were instead estimated from resilient-modulus tests with an artificial neural network, which by the guide’s own definition is a level 2 input; the software, however, only allowed entering calculated dynamic modulus through the level 1 option. Unbound materials were treated as level 2, with resilient modulus calculated from LTPP repeated-load test data using the NCHRP 1-28A approach. The lesson for a materials lab is that the input level a test result qualifies for depends on how it was produced, and that this should be reported with the result.
Field deflection testing and backcalculation
Backcalculation of layer moduli from deflection data is the bridge between field tests and design inputs. FHWA’s RD-97-091 TechBrief and RD-97-076 pamphlet describe a backcalculation procedure, based on ASTM D5858 and the LTPP procedure, that supports use of the 1993 AASHTO guide for flexible pavements. The same logic appears in the 2018 calibration: backcalculated moduli were converted to lab-equivalent values using C-values before use as unbound-layer inputs.
Climate, traffic and structure inputs
In the same calibration the climate data came from historical climate files in which each LTPP section had a corresponding climate station; water-table depth, which LTPP does not record, was set to a default of 5 m. Traffic inputs used two-way annual average daily truck traffic from LTPP monitoring tables, directional and lane factors of 100 percent, an operational speed of 100 km/h taken from the posted limit and compound growth. Layer thicknesses came from LTPP test records. These are the inputs a research team must be able to supply, defend and document when it produces a design analysis.
Foundation, drainage and economics
FHWA’s guidance adds design considerations beyond the structure itself. For fine-grained clay or silt subgrades it suggests considering stabilization of the upper 300 to 600 mm, and it encourages a 200 to 600 mm granular subbase on National Highway System pavements. Drainage should be considered on all projects, because poor subsurface drainage is a major cause of distress, especially in concrete pavements. New and rehabilitated pavements should receive an engineering and economic evaluation of alternatives, including life-cycle cost analysis covering agency and user costs. The guidance also notes that skid-resistant surfaces should be provided on all projects. Soil identification and classification tests that supply foundation descriptions are discussed in the guides to ASTM D2488 and ASTM D6913.
Common misunderstandings about pavement design
- “There is one required federal method.” There is not. The regulation states a performance goal, and agencies choose their own procedure.
- “AASHTO guide” means one document. The 1993 guide is empirical; the M-E guide and its software are a different basis. Check which one a specification cites.
- Pavement design is the same as geometric design. Alignment and cross-section are a separate discipline from layer design.
- More testing always means a higher input level. As the calibration study shows, a value estimated from another test is a level 2 input even when it is entered through a level 1 field.
- Defaults are findings. Defaults such as a 20-year design life, a 2.7 m/km terminal IRI and 90 percent reliability were used in the calibration because they did not matter for calibrating the models; they are not recommendations for any particular project.
Frequently asked questions
What is pavement design?
It is the process of selecting the layered structure and materials of a pavement so it can carry forecast traffic safely and durably over a design period. In US highway practice the rule in 23 CFR 626.3 sets that performance goal and leaves the method to each State Highway Agency.
Which method do US states use?
FHWA states that the regulation does not prescribe one. An agency may use the AASHTO guide or another procedure supported by past performance or research. Which one applies to a given project is set by that agency’s own policy.
What is the difference between the AASHTO 1993 guide and mechanistic-empirical design?
The 1993 guide uses empirical equations from the 1958 to 1960 AASHO Road Test. M-E design models damage accumulation over the service life from traffic, climate, materials and structure, and predicts distress and smoothness.
What distresses does M-E design predict?
For flexible pavements, longitudinal, alligator and transverse cracking and rutting. For rigid pavements, faulting, cracking and CRCP punch-outs. Smoothness is predicted for both.
Does this page give pavement thicknesses or design steps?
No. Thicknesses and steps depend on the adopted method, local calibration and the project, and are for the responsible engineer.
Sources
- FHWA, Pavement Design Considerations (formerly Non-Regulatory Supplement to 23 CFR 626), read 2026-11-20.
- 23 CFR 626.3 Policy, Cornell Legal Information Institute, read 2026-11-20.
- FHWA Focus, September 2004: the NCHRP 1-37A Mechanistic-Empirical Pavement Design Guide, read 2026-11-20.
- FHWA-HRT-17-104, Chapter 3, AASHTOWare Pavement ME Design calibration inputs, read 2026-11-20.
- FHWA-RD-97-091 TechBrief on backcalculation of layer moduli, read 2026-11-20.
Data: Pavement ME Design inputs and defaults used in FHWA's LTPP rutting calibration (version 2.2)
Compiled from FHWA-HRT-17-104 chapter 3: for each input category of the AASHTOWare Pavement ME Design rutting calibration, the value or source used and the input level or note stated in the report.
Period covered: 2018. Coverage: United States.
| Input category | Value or source used | Input level or note |
|---|---|---|
| Software version | AASHTOWare Pavement ME Design 2.2 | Rutting models calibrated for new and overlaid flexible pavements |
| Design life | 20 years (software default) | Adequate because rutting data were about 19 years after surface construction |
| Asphalt layer properties | Laboratory binder, volumetric, dynamic modulus, creep compliance data | Level 1 wherever data were available |
| Dynamic modulus | LTPP neural-network estimates from resilient modulus tests | Level 2 by definition; entered via the level 1 option |
| Unbound resilient modulus | Calculated from LTPP repeated-load tests (NCHRP 1-28A approach) | Level 2 |
| Terminal IRI | 2.7 m/km (default) | Not significant for calibration |
| Initial IRI | 1 m/km (default) | Not significant for calibration |
| Total permanent deformation limit | 19 mm (default) | Not significant for calibration |
| Asphalt-only deformation limit | 6 mm (default) | Not significant for calibration |
| Design reliability | 90 percent per criterion (default) | Not significant for calibration |
| Water table depth | 5 m default | Not recorded in LTPP |
| Directional and lane factors | 100 percent | Used for all sections |
| Operational speed | 100 km/h | From posted limit |
| Traffic growth | Compound | Assumed |
Sources
- FHWA-HRT-17-104 chapter 3 (accessed 2026-11-20)
Compiled by CASRAI from the sources above. Free to reuse under CC BY 4.0 with attribution.